Tyne and Wear · England

Crack stitching in Tyne and Wear

Crack stitching in Tyne and Wear starts with the ground. Clay soils are found in parts of Tyne and Wear, and the buildings here are mostly Tyneside flats and terraces, so the repair has to suit both.

Guide price from£75per metre of crack inc VAT

Close-up of stainless helical bars set into raked-out mortar joints across a crack
Area
Tyne and Wear
Pricing region
North East
Ground
Clay in parts
Towns listed
9

What should you know about the ground under Tyne and Wear?

Tyne and Wear lies on the Durham and Northumberland coalfield, with old shallow workings recorded beneath parts of Newcastle, Gateshead and Sunderland, mostly under a cover of glacial clay.

Historic coal workings are recorded beneath parts of Tyne and Wear, and a coal mining search is worth checking where movement is unexplained. Typical buildings in Tyne and Wear: Tyneside flats and terraces, Victorian villas, inter-war council estates and post-war semis.

How much will crack stitching cost in Tyne and Wear?

Guide prices below are for homes in Tyne and Wear, on North East rates and including VAT. A survey or good photos let us turn them into a fixed written price.

Guide prices inc VAT on North East rates. Items marked est. are our estimates.
ItemGuide pricePer
Crack stitching with stainless helical bars£75 – £165per metre of crack
Small jobs (minimum visit)est.£320 – £460per visit
Repointing over the stitched line in matching mortarest.£30 – £55per metre

Which repair method suits a home in Tyne and Wear?

Helical bars in cementitious grout

The most common approach. A slot is cut along the bed joint with a twin-blade cutter, flushed out and part filled with a cement-based grout. The helical bar is pushed in, more grout is packed over it, and the joint is pointed to match. The grout cures over a few days.

Best for: Most brick and block walls, including older softer bricks

Helical bars in resin grout

A resin grout bonds quickly and strongly to the bar and masonry and suits wet conditions or work that must take load sooner. It is less forgiving of soft or crumbly bricks, so the choice of grout is made wall by wall rather than as a rule.

Best for: Dense bricks, damp walls and repairs needing a fast cure

Stitching with crack injection

Once the bars are in, the crack itself is filled. Fine cracks are pointed in matching mortar, while wider or deeper cracks can be injected with grout so the void inside the wall is filled rather than just the face. On older houses, lime mortar keeps the repair breathable.

Best for: Deep cracks running through the full thickness of the wall

What happens when we carry out crack stitching in Tyne and Wear?

  1. Set out the bars

    Bar positions are marked across the crack, typically every few courses up its full height, with each bar extending well into sound brickwork on both sides. An engineer’s specification, where there is one, sets the exact spacing and length.

  2. Cut, clean and grout

    Slots are cut into the bed joints to the right depth, dust is blown and washed out, and grout is placed. The bars are pressed home and covered, and the crack line is filled or injected.

  3. Repoint to match

    The cut joints and crack are pointed in a mortar chosen to match the colour, texture and strength of the existing work. On older houses with soft bricks, a lime mortar is used so the repair does not trap moisture.

Signs you may need crack stitching

  • A crack you can fit a coin into, running through bricks and mortar
  • Bricks split clean through where the crack crosses them
  • Filled cracks that keep reopening along the same line
  • A crack visible on both the inside and outside face of the wall
Crack stitching: stainless helical bars grouted into bed joints across the crackBAR SPANS THE CRACKBED JOINT SLOT+ GROUTINDICATIVE · NOT TO SCALE
Crack stitching: stainless helical bars grouted into bed joints across the crack. Indicative drawing, not to scale.

Do you need approval for crack stitching in England?

Like-for-like repairs such as crack stitching and repointing do not usually need building control approval in England, but anything that changes or strengthens the structure, such as underpinning or rebuilding a wall, does. If the work touches a party wall, the Party Wall etc. Act 1996 may apply.

Crack stitching near you in Tyne and Wear

Crack stitching in Tyne and Wear: questions and answers

Does the ground around Newcastle upon Tyne cause cracking?

Tyne and Wear lies on the Durham and Northumberland coalfield, with old shallow workings recorded beneath parts of Newcastle, Gateshead and Sunderland, mostly under a cover of glacial clay. Historic coal workings are recorded beneath parts of Tyne and Wear, and a coal mining search is worth checking where movement is unexplained. Only an investigation on site can say why a particular building has moved.

How much will crack stitching cost in Tyne and Wear?

On North East rates, crack stitching starts from about £75 per metre of crack, including VAT. The written price depends on the extent of the damage, access and whether an engineer or building control is needed.

How far apart are helical bars placed?

Helical bars are usually placed every few courses up the full height of the crack, each one running well past the crack into sound brickwork. Spacing and bar length depend on the wall and the crack width, and where an engineer has specified the repair, their drawing sets them.

Can crack stitching be done from outside only?

Often yes, especially on cavity walls where only the outer leaf has cracked. On solid walls, or where the crack shows clearly inside, bars may be needed on both faces to reconnect the full thickness. We check both sides before quoting.

Does crack stitching stop a wall moving?

No, crack stitching reconnects cracked masonry but does not stop the movement that caused it. If the ground is still shrinking, a drain is still leaking or ties are still rusting, a stitched wall can crack again nearby. The cause has to be identified and dealt with first.

More repairs we carry out in Tyne and Wear

Next step

Send us photos of the crack or movement

A free initial assessment from your photos, then a no-obligation written quote. If an engineer, drain survey or monitoring is needed first, we say so before you spend anything.

CallGet a quote