Structural repairs across England, Wales, mainland Scotland and Northern Ireland · Free initial assessment from your photos0800 088 6341

Somerset · England

Crack stitching in Somerset

Across Somerset, requests for crack stitching usually begin with a crack someone has noticed getting wider. Parts of Somerset have clay that can shrink near trees in dry spells. A repair only lasts if the reason for the movement has stopped.

Guide price from£80per metre of crack inc VAT

Close-up of stainless helical bars set into raked-out mortar joints across a crack
Area
Somerset
Pricing region
South West
Ground
Clay in parts
Towns listed
11

Why does the ground in Somerset matter for crack stitching?

Somerset mixes Lias clays, Mercia Mudstone, limestone hills and the peat and alluvium of the Levels around Bridgwater, which can settle. The former Somerset coalfield around Radstock and Midsomer Norton left recorded workings.

Parts of Somerset lie on a former coalfield, so a coal mining search is worth checking if movement has no obvious cause. What you mostly find across Somerset: Bath stone Georgian terraces, Victorian houses in Taunton and Weston-super-Mare, and post-war estates.

What to expect when we carry out crack stitching

  1. Confirm the cause has stopped

    Before quoting we check what made the wall crack and whether it is still moving. If there is doubt, we suggest a period of monitoring or an engineer’s view, rather than stitching a crack that will simply open again.

  2. Cut, clean and grout

    Slots are cut into the bed joints to the right depth, dust is blown and washed out, and grout is placed. The bars are pressed home and covered, and the crack line is filled or injected.

  3. Repoint to match

    The cut joints and crack are pointed in a mortar chosen to match the colour, texture and strength of the existing work. On older houses with soft bricks, a lime mortar is used so the repair does not trap moisture.

Is it time for crack stitching? Common signs

  • Bricks split clean through where the crack crosses them
  • A crack visible on both the inside and outside face of the wall
  • Cracking that a surveyor or engineer has said is now stable
  • A crack you can fit a coin into, running through bricks and mortar

What should you budget for crack stitching in Somerset?

The ranges below reflect typical South West costs for crack stitching, including VAT. Scaffold, access and making good can push a job to the top of the range.

Guide prices inc VAT on South West rates. Items marked est. are our estimates.
ItemGuide pricePer
Crack stitching with stainless helical bars£80 – £185per metre of crack
Small jobs (minimum visit)est.£360 – £515per visit
Repointing over the stitched line in matching mortarest.£30 – £60per metre

Repair options we may recommend

Helical bars in resin grout

A resin grout bonds quickly and strongly to the bar and masonry and suits wet conditions or work that must take load sooner. It is less forgiving of soft or crumbly bricks, so the choice of grout is made wall by wall rather than as a rule.

Best for: Dense bricks, damp walls and repairs needing a fast cure

Helical bars in cementitious grout

The most common approach. A slot is cut along the bed joint with a twin-blade cutter, flushed out and part filled with a cement-based grout. The helical bar is pushed in, more grout is packed over it, and the joint is pointed to match. The grout cures over a few days.

Best for: Most brick and block walls, including older softer bricks

Stitching with crack injection

Once the bars are in, the crack itself is filled. Fine cracks are pointed in matching mortar, while wider or deeper cracks can be injected with grout so the void inside the wall is filled rather than just the face. On older houses, lime mortar keeps the repair breathable.

Best for: Deep cracks running through the full thickness of the wall

Crack stitching: stainless helical bars grouted into bed joints across the crackBAR SPANS THE CRACKBED JOINT SLOT+ GROUTINDICATIVE · NOT TO SCALE
Crack stitching: stainless helical bars grouted into bed joints across the crack. Indicative drawing, not to scale.

Do you need approval for crack stitching in England?

Like-for-like repairs such as crack stitching and repointing do not usually need building control approval in England, but anything that changes or strengthens the structure, such as underpinning or rebuilding a wall, does. If the work touches a party wall, the Party Wall etc. Act 1996 may apply.

Towns in Somerset we cover for crack stitching

Your crack stitching questions

Is the ground in Somerset prone to subsidence?

Somerset mixes Lias clays, Mercia Mudstone, limestone hills and the peat and alluvium of the Levels around Bridgwater, which can settle. The former Somerset coalfield around Radstock and Midsomer Norton left recorded workings. Parts of Somerset lie on a former coalfield, so a coal mining search is worth checking if movement has no obvious cause. Only an investigation on site can say why a particular building has moved.

How much will crack stitching cost in Somerset?

On South West rates, crack stitching starts from about £80 per metre of crack, including VAT. The written price depends on the extent of the damage, access and whether an engineer or building control is needed.

Does crack stitching stop a wall moving?

No, crack stitching reconnects cracked masonry but does not stop the movement that caused it. If the ground is still shrinking, a drain is still leaking or ties are still rusting, a stitched wall can crack again nearby. The cause has to be identified and dealt with first.

Is resin or cement grout better for crack stitching?

Neither is better in every case. Cement-based grout suits most walls and is kinder to soft, older bricks, while resin grout bonds faster and copes better with damp. The choice depends on the masonry, the conditions and any engineer’s specification.

How far apart are helical bars placed?

Helical bars are usually placed every few courses up the full height of the crack, each one running well past the crack into sound brickwork. Spacing and bar length depend on the wall and the crack width, and where an engineer has specified the repair, their drawing sets them.

Other structural repairs in Somerset

Next step

Send us photos of the crack or movement

A free initial assessment from your photos, then a no-obligation written quote. If an engineer, drain survey or monitoring is needed first, we say so before you spend anything.