Structural repairs across England, Wales, mainland Scotland and Northern Ireland · Free initial assessment from your photos0800 088 6341

Frome · Somerset

Crack stitching in Frome

Before we stitch a crack at a Frome property, we want to know why it opened and whether it has stopped. Stitching a wall that is still moving rarely holds, so the cause comes first and the bars come second.

Guide price from£80per metre of crack inc VAT

Close-up of stainless helical bars set into raked-out mortar joints across a crack
Postcodes
BA11
Population
about 26,000
Area
Somerset
Pricing region
South West

What should you know about the ground under Frome?

Frome (BA11) has around 26,000 residents and sits in Somerset. If you are just outside Frome, we also cover Westbury (6 miles), Warminster (6 miles) and Trowbridge (8 miles).

Parts of Somerset have clay that can shrink near trees in dry spells. Parts of Somerset lie on a former coalfield, so a coal mining search is worth checking if movement has no obvious cause. What you mostly find across Somerset: Bath stone Georgian terraces, Victorian houses in Taunton and Weston-super-Mare, and post-war estates.

Symptoms that point to crack stitching

  • Filled cracks that keep reopening along the same line
  • Cracking that a surveyor or engineer has said is now stable
  • A crack you can fit a coin into, running through bricks and mortar

Guide prices for crack stitching in Frome

For Frome we use South West rates. Treat the table as a budget guide, inc VAT; the price you pay is the one on your written quote.

Guide prices inc VAT on South West rates. Items marked est. are our estimates.
ItemGuide pricePer
Crack stitching with stainless helical bars£80 – £185per metre of crack
Small jobs (minimum visit)est.£360 – £515per visit
Repointing over the stitched line in matching mortarest.£30 – £60per metre

Methods for crack stitching

Stitching with crack injection

Once the bars are in, the crack itself is filled. Fine cracks are pointed in matching mortar, while wider or deeper cracks can be injected with grout so the void inside the wall is filled rather than just the face. On older houses, lime mortar keeps the repair breathable.

Best for: Deep cracks running through the full thickness of the wall

Helical bars in cementitious grout

The most common approach. A slot is cut along the bed joint with a twin-blade cutter, flushed out and part filled with a cement-based grout. The helical bar is pushed in, more grout is packed over it, and the joint is pointed to match. The grout cures over a few days.

Best for: Most brick and block walls, including older softer bricks

From first photo to finished repair

  1. Confirm the cause has stopped

    Before quoting we check what made the wall crack and whether it is still moving. If there is doubt, we suggest a period of monitoring or an engineer’s view, rather than stitching a crack that will simply open again.

  2. Repoint to match

    The cut joints and crack are pointed in a mortar chosen to match the colour, texture and strength of the existing work. On older houses with soft bricks, a lime mortar is used so the repair does not trap moisture.

  3. Make good and record

    Internal plaster cracks are cut out and filled where included, and dust is cleared. You receive a short note of where the bars went, which is useful for future buyers, surveyors and any insurance file.

Rules for crack stitching in England

Like-for-like repairs such as crack stitching and repointing do not usually need building control approval in England, but anything that changes or strengthens the structure, such as underpinning or rebuilding a wall, does. If the work touches a party wall, the Party Wall etc. Act 1996 may apply.

Frequently asked questions

What is the price of crack stitching in Frome?

Guide prices for crack stitching in Frome start from about £80 per metre of crack, including VAT, on South West rates. Your fixed written price follows photos or a survey and depends on the extent of the work and access.

Do you carry out crack stitching in Frome?

We do. Frome and the surrounding area are covered, including nearby Westbury and Warminster. A free initial assessment from your photos is the first step.

Does the ground around Frome cause cracking?

Somerset mixes Lias clays, Mercia Mudstone, limestone hills and the peat and alluvium of the Levels around Bridgwater, which can settle. The former Somerset coalfield around Radstock and Midsomer Norton left recorded workings. Only an investigation can say why a particular building has moved.

Does crack stitching stop a wall moving?

No, crack stitching reconnects cracked masonry but does not stop the movement that caused it. If the ground is still shrinking, a drain is still leaking or ties are still rusting, a stitched wall can crack again nearby. The cause has to be identified and dealt with first.

How far apart are helical bars placed?

Helical bars are usually placed every few courses up the full height of the crack, each one running well past the crack into sound brickwork. Spacing and bar length depend on the wall and the crack width, and where an engineer has specified the repair, their drawing sets them.

More repairs we carry out in Frome

Crack stitching near Frome

Hold a ruler against the crack at your Frome home, take a clear photo and send it in for a free initial assessment and a guide price.

Next step

Send us photos of the crack or movement

A free initial assessment from your photos, then a no-obligation written quote. If an engineer, drain survey or monitoring is needed first, we say so before you spend anything.

CallGet a quote