What should you know about the ground under West Sussex?
North West Sussex around Crawley and Horsham sits on Weald Clay, the South Downs are chalk, and the coastal plain has brickearth and gravels. The Weald Clay is prone to shrink-swell movement near trees.
Ground movement here is more often linked to soils, drains and trees than to mining. Across West Sussex, most homes are Wealden cottages, 1930s semis and bungalows on the coast, and new-town estates in Crawley.
Symptoms that point to crack stitching
- A crack you can fit a coin into, running through bricks and mortar
- Filled cracks that keep reopening along the same line
- A crack visible on both the inside and outside face of the wall
- Bricks split clean through where the crack crosses them
Guide prices for crack stitching in West Sussex
For West Sussex we use South East rates. Treat the table as a budget guide, inc VAT; the price you pay is the one on your written quote.
| Item | Guide price | Per |
|---|---|---|
| Crack stitching with stainless helical bars | £90 – £200 | per metre of crack |
| Small jobs (minimum visit)est. | £390 – £560 | per visit |
| Repointing over the stitched line in matching mortarest. | £35 – £65 | per metre |
Methods for crack stitching
Helical bars in resin grout
A resin grout bonds quickly and strongly to the bar and masonry and suits wet conditions or work that must take load sooner. It is less forgiving of soft or crumbly bricks, so the choice of grout is made wall by wall rather than as a rule.
Best for: Dense bricks, damp walls and repairs needing a fast cure
Stitching with crack injection
Once the bars are in, the crack itself is filled. Fine cracks are pointed in matching mortar, while wider or deeper cracks can be injected with grout so the void inside the wall is filled rather than just the face. On older houses, lime mortar keeps the repair breathable.
Best for: Deep cracks running through the full thickness of the wall
Helical bars in cementitious grout
The most common approach. A slot is cut along the bed joint with a twin-blade cutter, flushed out and part filled with a cement-based grout. The helical bar is pushed in, more grout is packed over it, and the joint is pointed to match. The grout cures over a few days.
Best for: Most brick and block walls, including older softer bricks
From first photo to finished repair
Confirm the cause has stopped
Before quoting we check what made the wall crack and whether it is still moving. If there is doubt, we suggest a period of monitoring or an engineer’s view, rather than stitching a crack that will simply open again.
Cut, clean and grout
Slots are cut into the bed joints to the right depth, dust is blown and washed out, and grout is placed. The bars are pressed home and covered, and the crack line is filled or injected.
Repoint to match
The cut joints and crack are pointed in a mortar chosen to match the colour, texture and strength of the existing work. On older houses with soft bricks, a lime mortar is used so the repair does not trap moisture.
Do you need approval for crack stitching in England?
Like-for-like repairs such as crack stitching and repointing do not usually need building control approval in England, but anything that changes or strengthens the structure, such as underpinning or rebuilding a wall, does. If the work touches a party wall, the Party Wall etc. Act 1996 may apply.
Towns in West Sussex we cover for crack stitching
- Crawley
- Worthing
- Bognor Regis
- Littlehampton
- Horsham
- Haywards Heath
- Chichester
- Burgess Hill
- East Grinstead
- Shoreham-by-Sea
- Lancing
Frequently asked questions
Is the ground in West Sussex prone to subsidence?
North West Sussex around Crawley and Horsham sits on Weald Clay, the South Downs are chalk, and the coastal plain has brickearth and gravels. The Weald Clay is prone to shrink-swell movement near trees. Ground movement here is more often linked to soils, drains and trees than to mining. Only an investigation on site can say why a particular building has moved.
How much will crack stitching cost in West Sussex?
On South East rates, crack stitching starts from about £90 per metre of crack, including VAT. The written price depends on the extent of the damage, access and whether an engineer or building control is needed.
Is resin or cement grout better for crack stitching?
Neither is better in every case. Cement-based grout suits most walls and is kinder to soft, older bricks, while resin grout bonds faster and copes better with damp. The choice depends on the masonry, the conditions and any engineer’s specification.
Can crack stitching be done from outside only?
Often yes, especially on cavity walls where only the outer leaf has cracked. On solid walls, or where the crack shows clearly inside, bars may be needed on both faces to reconnect the full thickness. We check both sides before quoting.
How far apart are helical bars placed?
Helical bars are usually placed every few courses up the full height of the crack, each one running well past the crack into sound brickwork. Spacing and bar length depend on the wall and the crack width, and where an engineer has specified the repair, their drawing sets them.