Egham · Surrey
Concrete repairs in Egham
Where flats and houses in Egham and across Surrey have concrete balconies, canopies or lintels several decades old, carbonation has had time to reach the reinforcement. That is when spalling and straight-line cracking tend to appear.
Guide price from£95per m² inc VAT

- Postcodes
- TW20
- Population
- about 30,000
- Area
- Surrey
- Pricing region
- South East
What is the ground like in Surrey?
Egham (TW20) has around 30,000 residents and sits in Surrey. Neighbouring towns we cover: Staines-upon-Thames (2 miles), Chertsey (4 miles) and Ashford (4 miles).
Shrinkable clay is widespread in Surrey. Ground movement here is more often linked to soils, drains and trees than to mining. Housing stock in Surrey: Victorian and Edwardian villas, 1930s semis and detached houses in the commuter towns, and post-war estates.
Symptoms that point to concrete repairs
- Exposed steel bars showing where concrete has fallen away
- Hollow sound when the surface is tapped with a hammer
- Rust-coloured stains or streaks running down the concrete surface
Guide prices for concrete repairs in Egham
Prices in Egham are worked out on South East rates. They include VAT and are a starting point: access, the extent of the damage and whether an engineer or building control is involved all move the figure.
| Item | Guide price | Per |
|---|---|---|
| Concrete patch repair | £95 – £200 | per m² |
| Crack injection | £200 – £540 | per metre |
| Small jobs (minimum visit)est. | £505 – £1,000 | per visit |
Methods for concrete repairs
Patch repair
Loose and contaminated concrete is broken out behind the bar, the steel is cleaned of rust and primed, and the section is rebuilt with a repair mortar. The edges are cut square so the patch does not feather out and fail. A protective coating may be applied over the whole surface afterwards.
Best for: Localised spalling around rusting bars
Protective coatings and sealing
After repair, an anti-carbonation coating, a waterproof deck membrane on a balcony, or a penetrating sealer slows the return of moisture and carbon dioxide. Restoring drips, upstands and falls so water drains away is as important as the coating itself.
Best for: Extending the life of repaired balconies and canopies
From first photo to finished repair
Survey and tapping test
On site we tap the surface to find hollow areas, check the steel where it is exposed and note drainage. Where the extent is unclear, a cover meter, carbonation test or chloride test may be advised before repair.
Engineer where needed
If the steel has lost significant section, or the element carries a balcony, stair or wall, an independent chartered structural engineer is appointed to assess and specify. We can arrange this, and the repair follows their scope.
Break out, repair, protect
Damaged concrete is cut back to sound material, steel cleaned and primed, and the section rebuilt and cured. Cracks are injected, then the surface is coated and drainage details put right so water runs off rather than sitting.
Rules for concrete repairs in England
Like-for-like repairs such as crack stitching and repointing do not usually need building control approval in England, but anything that changes or strengthens the structure, such as underpinning or rebuilding a wall, does. If the work touches a party wall, the Party Wall etc. Act 1996 may apply.
Frequently asked questions
How much will concrete repairs cost in Egham?
Guide prices for concrete repairs in Egham start from about £95 per m², including VAT, on South East rates. Your fixed written price follows photos or a survey and depends on the extent of the work and access.
Do you cover Egham?
We do. Egham and the surrounding area are covered, including nearby Staines-upon-Thames and Chertsey. A free initial assessment from your photos is the first step.
Is the ground in Surrey prone to subsidence?
North Surrey sits on London Clay, the south on Weald Clay, with chalk along the North Downs and sands in the west. Large gardens with mature trees on clay make seasonal subsidence a familiar problem. Only an investigation can say why a particular building has moved.
Is spalling concrete dangerous?
It can be, mainly because pieces may fall from balconies, canopies and soffits above doors or paths. It also means the steel is losing strength over time. Fence off the area below any loose concrete, keep people off a balcony that is badly affected, and have it assessed soon.
What is carbonation in concrete?
Carbonation is the gradual reaction between carbon dioxide in the air and concrete, which lowers its alkalinity from the surface inward. Alkaline concrete protects the steel inside, so when carbonation reaches the bars, they can start to rust. A simple test on a freshly broken surface shows how deep it has gone.
Other structural repairs in Egham
- Roof structure repairs
- Underpinning
- Structural surveys and crack monitoring
- Boundary and garden wall repairs
- Floor joist repairs
Concrete repairs near Egham
Send close-up and wide photos of the damaged concrete at your Egham property for a free initial assessment and a no-obligation written quote.