From a cracked canopy over a shop door to a spalling lintel on a house, concrete repairs in New Milton follow the same steps. Cut back to sound concrete, treat the steel, rebuild the section and stop water getting back in.
Guide price from£95per m² inc VAT

- Postcodes
- BH25
- Population
- about 26,000
- Area
- Hampshire
- Pricing region
- South East
What is the ground like in Hampshire?
With roughly 26,000 people, New Milton spans postcode districts BH25 in Hampshire. Neighbouring towns we cover: Christchurch (5 miles), Bournemouth (10 miles) and Ferndown (11 miles).
Shrinkable clay is widespread in Hampshire. Ground movement here is more often linked to soils, drains and trees than to mining. Housing stock in Hampshire: Victorian terraces in Portsmouth and Southampton, 1930s semis, and large post-war and new-build estates.
Symptoms that point to concrete repairs
- Fine cracks running in straight lines along the line of the reinforcement
- Chunks or flakes of concrete breaking away from edges and soffits
- Rust-coloured stains or streaks running down the concrete surface
Guide prices for concrete repairs in New Milton
Guide prices below are for homes in New Milton, on South East rates and including VAT. A survey or good photos let us turn them into a fixed written price.
| Item | Guide price | Per |
|---|---|---|
| Concrete patch repair | £95 – £200 | per m² |
| Crack injection | £200 – £540 | per metre |
| Small jobs (minimum visit)est. | £505 – £1,000 | per visit |
Methods for concrete repairs
Patch repair
Loose and contaminated concrete is broken out behind the bar, the steel is cleaned of rust and primed, and the section is rebuilt with a repair mortar. The edges are cut square so the patch does not feather out and fail. A protective coating may be applied over the whole surface afterwards.
Best for: Localised spalling around rusting bars
Protective coatings and sealing
After repair, an anti-carbonation coating, a waterproof deck membrane on a balcony, or a penetrating sealer slows the return of moisture and carbon dioxide. Restoring drips, upstands and falls so water drains away is as important as the coating itself.
Best for: Extending the life of repaired balconies and canopies
From first photo to finished repair
Survey and tapping test
On site we tap the surface to find hollow areas, check the steel where it is exposed and note drainage. Where the extent is unclear, a cover meter, carbonation test or chloride test may be advised before repair.
Engineer where needed
If the steel has lost significant section, or the element carries a balcony, stair or wall, an independent chartered structural engineer is appointed to assess and specify. We can arrange this, and the repair follows their scope.
Break out, repair, protect
Damaged concrete is cut back to sound material, steel cleaned and primed, and the section rebuilt and cured. Cracks are injected, then the surface is coated and drainage details put right so water runs off rather than sitting.
Rules for concrete repairs in England
Like-for-like repairs such as crack stitching and repointing do not usually need building control approval in England, but anything that changes or strengthens the structure, such as underpinning or rebuilding a wall, does. If the work touches a party wall, the Party Wall etc. Act 1996 may apply.
Frequently asked questions
How much should I budget for concrete repairs in New Milton?
Guide prices for concrete repairs in New Milton start from about £95 per m², including VAT, on South East rates. Your fixed written price follows photos or a survey and depends on the extent of the work and access.
Can you survey a property in New Milton?
Yes, New Milton is covered, along with postcode districts BH25. We also cover nearby Christchurch and Bournemouth.
Why do houses in Hampshire crack?
Central Hampshire is chalk, while the south around Portsmouth, Southampton and the New Forest fringe and the north-east around Farnborough sit on London Clay, Reading Beds and other clays and sands. The clay areas see seasonal movement near trees. Only an investigation can say why a particular building has moved.
What is spalling concrete?
Spalling is concrete breaking away from the surface in flakes or chunks. In reinforced concrete it is usually caused by the steel inside rusting and expanding, which pushes the cover off. It often follows a straight line where a bar sits close to the surface, with rust staining nearby.
Why does concrete crack and rust?
Concrete cracks as it shrinks, moves with temperature or carries more load than intended. Steel inside it rusts when carbonation or salts reach it and moisture gets in. The two feed each other: cracks let water in, and rusting steel expands and cracks the concrete further.