If you have found a crack in a wall at your Saltash property, the first job is to work out why it appeared. Our crack repairs start with the cause, so the stitching, repointing or rebuilding that follows has a fair chance of lasting.

Guide price from£80per metre of crack inc VAT

Repointing fresh mortar into a repaired diagonal crack in old brickwork
Postcodes
PL12
Population
about 16,000
Area
Cornwall
Pricing region
South West

Is Cornwall prone to ground movement?

Postcode districts PL12 cover Saltash, a Cornwall town of about 16,000 people. If you are just outside Saltash, we also cover Plymouth (4 miles), Bodmin (22 miles) and St Austell (25 miles).

Shrinkable clay is less common in Cornwall than in south-east England. Old metal-mine shafts and workings are recorded in places, so mining searches are routine for some properties. Typical buildings in Cornwall: Granite and slate-stone cottages, cob buildings, Victorian terraces and post-war estates.

From first photo to finished repair

  1. Survey and record

    On site we measure the width along the crack, note its pattern and check nearby drains, trees and openings. If the cause is unclear, gauges can be fixed across it and read over several months.

  2. Deal with the cause

    Leaking drains, failed ties, a sagging lintel or ground movement are put right first, sometimes through an insurance claim. Repairing a crack before its cause is fixed usually means paying for the same job twice.

  3. Written quote

    You receive a no-obligation written quote listing each crack, the repair method chosen for it and the making good inside and out. Once the scope is settled, that becomes a fixed price in writing.

Symptoms that point to structural crack repairs

  • Diagonal cracks running from the corners of windows and doors
  • Stepped cracks zigzagging through the mortar joints of outside brickwork
  • Daylight or a draught coming through a crack in an outside wall

Guide prices for structural crack repairs in Saltash

Guide prices below are for homes in Saltash, on South West rates and including VAT. A survey or good photos let us turn them into a fixed written price.

Guide prices inc VAT on South West rates. Items marked est. are our estimates.
ItemGuide pricePer
Crack stitching with helical bars£80 – £185per metre of crack
Single crack, outside only (up to about 2 m)est.£410 – £925per crack
Internal making good and redecoration of the crack lineest.£155 – £515per room

Methods for structural crack repairs

Crack stitching with helical bars

Stainless steel helical bars are grouted into slots cut along the bed joints, bridging the crack so the masonry works as one piece again. It is the standard repair for wider stepped and vertical cracks once whatever caused them has stopped.

Best for: Stable cracks wider than about 5 mm, or ones that keep reopening

Filling and repointing

For hairline and narrow cracks that have stopped moving, the crack line is raked out and repointed in mortar matched to the original for strength, colour and texture. Inside, plaster cracks are cut out, filled with a flexible filler and redecorated.

Best for: Cracks up to about 5 mm that are no longer moving

Rules for structural crack repairs in England

Like-for-like repairs such as crack stitching and repointing do not usually need building control approval in England, but anything that changes or strengthens the structure, such as underpinning or rebuilding a wall, does. If the work touches a party wall, the Party Wall etc. Act 1996 may apply.

Frequently asked questions

What is the price of structural crack repairs in Saltash?

Guide prices for structural crack repairs in Saltash start from about £80 per metre of crack, including VAT, on South West rates. Your fixed written price follows photos or a survey and depends on the extent of the work and access.

Do you carry out structural crack repairs in Saltash?

Yes. We take enquiries from across Saltash, including PL12, and from nearby places such as Plymouth and Bodmin. Send photos for a free initial view and we will tell you what happens next.

Does the ground around Saltash cause cracking?

Cornwall is mostly granite and slate with little shrinkable clay, so clay subsidence is less common than in the south-east. Historic tin and copper mining has left shafts and workings in places such as Camborne and Redruth, and mining searches are routine there. Only an investigation can say why a particular building has moved.

What causes vertical cracks in walls?

Vertical cracks are most often caused by thermal or moisture movement in long walls, or by the joint between old and newer work. An even-width vertical crack is usually cosmetic. One clearly wider at the top or bottom can indicate foundation movement at one end.

What do stepped cracks in brickwork mean?

Stepped cracks usually mean part of the wall has moved and the weakest path, the mortar joints, has given way. They are common with subsidence and around openings. A thin stepped crack unchanged for years is often cosmetic, while a wide or tapered one should be looked at.

More repairs we carry out in Saltash

Structural crack repairs near Saltash

Each crack at your Saltash property is priced separately in our written quote, so you can see exactly what you are paying for and why.

Next step

Send us photos of the crack or movement

A free initial assessment from your photos, then a no-obligation written quote. If an engineer, drain survey or monitoring is needed first, we say so before you spend anything.

CallGet a quote