Stitched repairs suit most brick and block walls in Gloucester, from older solid nine-inch walls to modern cavity construction. On soft historic brick we use lime mortar and grout chosen to suit it, so the repair does not damage the wall.

Guide price from£80per metre of crack inc VAT

Close-up of stainless helical bars set into raked-out mortar joints across a crack
Postcodes
GL1, GL2, GL4
Population
about 130,000
Area
Gloucestershire
Pricing region
South West

What is the ground like in Gloucestershire?

With roughly 130,000 people, Gloucester spans postcode districts GL1, GL2, GL4 in Gloucestershire. Nearby places we cover include Cheltenham (7 miles), Stroud (8 miles) and Tewkesbury (9 miles).

Clay soils are found in parts of Gloucestershire. Parts of Gloucestershire lie on a former coalfield, so a coal mining search is worth checking if movement has no obvious cause. What you mostly find across Gloucestershire: Cotswold stone cottages, Regency terraces in Cheltenham, and brick estates around Gloucester.

Repair options we may recommend

Stitching with crack injection

Once the bars are in, the crack itself is filled. Fine cracks are pointed in matching mortar, while wider or deeper cracks can be injected with grout so the void inside the wall is filled rather than just the face. On older houses, lime mortar keeps the repair breathable.

Best for: Deep cracks running through the full thickness of the wall

Helical bars in resin grout

A resin grout bonds quickly and strongly to the bar and masonry and suits wet conditions or work that must take load sooner. It is less forgiving of soft or crumbly bricks, so the choice of grout is made wall by wall rather than as a rule.

Best for: Dense bricks, damp walls and repairs needing a fast cure

What to expect when we carry out crack stitching

  1. Confirm the cause has stopped

    Before quoting we check what made the wall crack and whether it is still moving. If there is doubt, we suggest a period of monitoring or an engineer’s view, rather than stitching a crack that will simply open again.

  2. Cut, clean and grout

    Slots are cut into the bed joints to the right depth, dust is blown and washed out, and grout is placed. The bars are pressed home and covered, and the crack line is filled or injected.

  3. Repoint to match

    The cut joints and crack are pointed in a mortar chosen to match the colour, texture and strength of the existing work. On older houses with soft bricks, a lime mortar is used so the repair does not trap moisture.

Is it time for crack stitching? Common signs

  • A crack visible on both the inside and outside face of the wall
  • Bricks split clean through where the crack crosses them
  • A crack you can fit a coin into, running through bricks and mortar

What should you budget for crack stitching in Gloucester?

For Gloucester we use South West rates. Treat the table as a budget guide, inc VAT; the price you pay is the one on your written quote.

Guide prices inc VAT on South West rates. Items marked est. are our estimates.
ItemGuide pricePer
Crack stitching with stainless helical bars£80 – £185per metre of crack
Small jobs (minimum visit)est.£360 – £515per visit
Repointing over the stitched line in matching mortarest.£30 – £60per metre

Rules for crack stitching in England

Like-for-like repairs such as crack stitching and repointing do not usually need building control approval in England, but anything that changes or strengthens the structure, such as underpinning or rebuilding a wall, does. If the work touches a party wall, the Party Wall etc. Act 1996 may apply.

Your crack stitching questions

What is the price of crack stitching in Gloucester?

Guide prices for crack stitching in Gloucester start from about £80 per metre of crack, including VAT, on South West rates. Your fixed written price follows photos or a survey and depends on the extent of the work and access.

Do you carry out crack stitching in Gloucester?

Yes. We take enquiries from across Gloucester, including GL1, GL2, GL4, and from nearby places such as Cheltenham and Stroud. Send photos for a free initial view and we will tell you what happens next.

Does the ground around Gloucester cause cracking?

The Severn vale around Gloucester, Cheltenham and Tewkesbury is Lias and Mercia Mudstone clay, the Cotswolds are limestone, and the Forest of Dean has a historic coalfield. Parts of South Gloucestershire around Kingswood also lie on old Coal Measures. Only an investigation can say why a particular building has moved.

Can I stitch a crack myself?

It is possible on a small, stable crack, but the work involves cutting into joints with a twin-blade cutter, controlling silica dust and placing the bars correctly. If the crack is part of an insurance claim or is wide, have it assessed first, because a poor repair can hide ongoing movement.

Can crack stitching be done from outside only?

Often yes, especially on cavity walls where only the outer leaf has cracked. On solid walls, or where the crack shows clearly inside, bars may be needed on both faces to reconnect the full thickness. We check both sides before quoting.

More repairs we carry out in Gloucester

Crack stitching near Gloucester

Hold a ruler against the crack at your Gloucester home, take a clear photo and send it in for a free initial assessment and a guide price.

Next step

Send us photos of the crack or movement

A free initial assessment from your photos, then a no-obligation written quote. If an engineer, drain survey or monitoring is needed first, we say so before you spend anything.

CallGet a quote